1·The blooming mill shop of wuhan Iron & Steel Co. want to reform its bloom shear for the purpose of increasing the shear force from 1600 metric ton to 2000 metric ton.
武钢初轧厂要求将其现有的1600吨双偏心浮动轴重锤平衡式钢坯剪改造为2000吨单偏心浮动轴液压平衡式。
2·The existing cooling ability of bloom continuous casting mold at PZH Steel was evaluated, then, the mold cooling process was optimized.
在分析攀钢大方坯连铸现行结晶器冷却能力的基础上,优化调整了结晶器冷却制度。
3·A variety of protective casting process have been developed for decreasing defect on killed steel bloom sur-face.
为了减少镇静钢钢锭(坯)表面缺陷,出现了各种类型的保护浇铸技术。
4·It is specified for applications in high temp. bloom-roll and other hot rolling of steel products to clear away scales.
此工艺适用于高温热轧钢坯及成品钢材的表面去除氧化铁皮。
5·The key technologies, such as M-EMS, secondary cooling scheme, and dynamic soft reduction, and its application to bloom continuous casting for heavy rail steel were presented.
简述了攀钢大方坯连铸结晶器电磁搅拌技术、二冷控制技术和凝固末端动态轻压下技术在重轨钢连铸中的应用效果。
6·The key technologies, such as M-EMS, secondary cooling scheme, dynamic soft reduction, and its application to bloom continuous casting for heavy rail steel were presented.
简述了攀钢大方坯连铸结晶器电磁搅拌技术、二冷控制技术和凝固末端动态轻压下技术在重轨钢连铸中的应用效果。
7·The basic control functions of RH vacuum installation for bloom CCM in PANGANG Iron & Steel Group Co. are presented, emphasizing the vacuum pump control system.
介绍攀钢方坯RH精炼装置真空系统基本控制功能,侧重介绍真空泵系统的功能和其相关系统控制。
8·With a bloom caster of steel factory as research background, the establishment of dynamic soft reduction zone model was introduced.
以某钢厂方坯连铸机为研究背景,介绍了建立动态轻压下压下区域模型的方法。
9·The refining technologies of liquid steel before it is poured into tube bloom on continuous casting machine are introduced.
介绍了连铸机浇铸管坯之前钢水的处理技术。
10·No quality round bloom, no quality seamless steel tube.
优质的圆管坯是生产高质量无缝钢管的前提。